Hello friends,

I infused a medium size part (1.30 x 0.40 meters) and say that 95% of the part was perfect, a small part was dry effect because the resin did not distribute perfectly.

Please, I would like a help, a solution to save this, because it generated me much expense and I would not like to infuse another part.

Suggestions to save the partwill be welcome.

Thanks