Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
General Composites Discussion
»
Repair
Repair
Post Reply
Like
3
Repair
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
111mattin111
111mattin111
posted 7 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 67,
Visits: 910
Hi guys what would be the best method to repair this to a high standard
Thanks Paul
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Repair
111mattin111
-
7 Years Ago
Has it gone through the lacquer to the fabric?
scottracing
-
7 Years Ago
No its not touched the fabric
111mattin111
-
7 Years Ago
If the fabric is ok then it is simply a case of removing the damaged clear coat and then respraying it. The hardest part is to do that without touching the fibres, but realistically even if you do...
Hanaldo
-
7 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search