By 111mattin111 - 2/15/2018 8:21:32 AM

Hi guys what would be the best method to repair this to a high standard 

Thanks Paul 
By Hanaldo - 2/17/2018 1:41:06 AM

If the fabric is ok then it is simply a case of removing the damaged clear coat and then respraying it. The hardest part is to do that without touching the fibres, but realistically even if you do take a bit off the fibres it won't stand out cosmetically unless you really chew into them.

You can also try applying a bit of very low viscosity resin to the cracks by dabbing them with a pop-stick, and this may reduce the amount of material you need to remove.