Warren (Staff) - 2/14/2018 3:47:09 PM
That laminate lay up should hold its shape pretty well.

In terms of resin infusion, EF80 is not designed for infusion and is a bit too thick.  An easier process would be wet lay vacuum bagging as you can use the vacuum consolidation to remove any  trapped air and excess resin..

Thanks. I'm gone use vacuum bagging for sure.

Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
That laminate lay up should hold its shape pretty well.

In terms of resin infusion, EF80 is not designed for infusion and is a bit too thick.  An easier process would be wet lay vacuum bagging as you can use the vacuum consolidation to remove any  trapped air and excess resin..


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Zemoleiro
Z
Forum Guru (66 reputation)Forum Guru (66 reputation)Forum Guru (66 reputation)Forum Guru (66 reputation)Forum Guru (66 reputation)Forum Guru (66 reputation)Forum Guru (66 reputation)Forum Guru (66 reputation)Forum Guru (66 reputation)
Group: Forum Members
Posts: 4, Visits: 20
Hi Easycomposites.

I'm planning to build some fender flares for an UTV, like the ones in the picture, using EF80 Flexible Epoxy Resin, and I have some questions about it.
The UTV is used in racing, so the fenders are exposed to impacts of rocks and branches of bushes at high speed.
I'm thinking in laminate the follow layers:
1x Carbon Fibre 2/2 Twill 200g.
2x Carbon Kevlar Plain Weave 188g.
1x Carbon Fibre 45' Biaxial 300g.
2x Carbon Kevlar Plain Weave 188g.
1x Carbon Black Twaron 2/2 Twill 200g. 
My questions are:
It's possible to do infusion with the EF80 Flexible Resin, to avoid to have air bubbles in the laminate (I want the piece to have a nice cosmetic presentation)?
With these layers, do you think that the fenders maintains the shape without deforming, or should I use some reinforcements in some areas ?
Thanks and regards
José Moleiro


GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search