Jaspen - 3/6/2018 1:19:02 AM
İlyas Məmmədzadə - 2/8/2018 8:03:05 AM
Hello Is it ok to wrap the bonnet with a transparent vinyl before starting the moulding?  In order not to damage the bonnet paint. 
thanks

Hello

Pleas don't. When you making molding. You will apply gel coat. Resin. Those material will give out heat in chemical reaction with heat. Those will make the vinyl holograms on yr hood. You need repaint yr hood! 3d scannng yr hood is recommended for yr.case! 

Like above, tried it before and the gelcoat weakened the vinyl making it soft and giving it some wrinkles...the curing of a mould can go up in temperatures till 70°C if thick lay up so this will soften the vinyl and glue as well... 
Like Hanaldo said above a PVA might make a barrierfilm to prevent the gelcoat softening the vinyl but heat will still be an issue...not saying it is impossible but take great care...I would personally rather go for the chemical release agent or pva straight on the hood and worst case you'll have to repaint the hood Smile


Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




Jaspen
Jaspen
Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)
Group: Forum Members
Posts: 9, Visits: 24
İlyas Məmmədzadə - 2/8/2018 8:03:05 AM
Hello Is it ok to wrap the bonnet with a transparent vinyl before starting the moulding?  In order not to damage the bonnet paint. 
thanks

Hello

Pleas don't. When you making molding. You will apply gel coat. Resin. Those material will give out heat in chemical reaction with heat. Those will make the vinyl holograms on yr hood. You need repaint yr hood! 3d scannng yr hood is recommended for yr.case! 
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
I think you need to be looking at what is going wrong then... Certainly plug damage is always possible, but it is far from impossible to avoid it. 
Jaspen
Jaspen
Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)
Group: Forum Members
Posts: 9, Visits: 24
Hanaldo - 2/9/2018 6:13:56 AM
It is fine as long as you are using PVA release agent. Otherwise the gelcoat will attack the vinyl. 

I am a bodykit manufacturer in HongKong. According to my 6 years experience on Hood molding. It was impossbile not to not
damage the bonnet paint for no matter what protections that you do!  Its just maybe damaged minor only!


Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
It is fine as long as you are using PVA release agent. Otherwise the gelcoat will attack the vinyl. 
İlyas Məmmədzadə
İlyas Məmmədzadə
Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)Junior Member (6 reputation)
Group: Forum Members
Posts: 1, Visits: 3
Hello Is it ok to wrap the bonnet with a transparent vinyl before starting the moulding?  In order not to damage the bonnet paint. 
thanks
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search