Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Equipment and Materials
»
Brain fart
Brain fart
Post Reply
Like
7
Brain fart
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
TonyW
T
TonyW
posted 8 Years Ago
ANSWER
HOT
Post Details
T
Group: Forum Members
Posts: 12,
Visits: 34
+
x
Warren (Staff) - 2/5/2018 9:25:02 AM
XCR is fine for hand laminating so you should be fine.
Cheers Warren. I couldn' wait so went ahead a did it anyway but unfortunately I trapped a stray piece of carbon under the resin and ruined the piece. Will do better next time though lol
Reply
Like
6
Warren (Staff)
Warren (Staff)
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
XCR is fine for hand laminating so you should be fine.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Reply
Like
7
TonyW
T
TonyW
posted 8 Years Ago
ANSWER
HOT
Topic Details
T
Group: Forum Members
Posts: 12,
Visits: 34
So I've ordered the wrong resin 😣 I'm doing a wet lay up so I should of ordered the el2 laminating resin but I accidentally ordered the xcr coating resin. Would this resin be alright to use for that as I really need to get this part made this weekend or will I be wasting time and materials?
Cheer Tonys
Reply
Like
7
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search