Talk Composites - The Forum for Advanced Composites
Home
»
Advanced Composites Forum
»
Equipment and Materials
Brain fart
http://www.talkcomposites.com/Topic25107.aspx
By TonyW
-
2/3/2018 11:42:05 AM
So I've ordered the wrong resin 😣 I'm doing a wet lay up so I should of ordered the el2 laminating resin but I accidentally ordered the xcr coating resin. Would this resin be alright to use for that as I really need to get this part made this weekend or will I be wasting time and materials?
Cheer Tonys
By TonyW
-
2/5/2018 10:02:47 AM
+
x
Warren (Staff) - 2/5/2018 9:25:02 AM
XCR is fine for hand laminating so you should be fine.
Cheers Warren. I couldn' wait so went ahead a did it anyway but unfortunately I trapped a stray piece of carbon under the resin and ruined the piece. Will do better next time though lol