Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Projects
»
Motorsport, Vehicle Design and Modification
»
New Design
New Design
Post Reply
Like
9
New Design
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Jossure
J
Jossure
posted 8 Years Ago
ANSWER
HOT
Topic Details
J
Group: Forum Members
Posts: 6,
Visits: 17
Hello all,
I am interested in designing my own car and about 3 weeks ago, I decided to start learning basic designs on Fusion 360 simply because it cost zero dollars. Given that I had never designed anything before using any computer design programs, I would like you to rate for me this car that I designed. Do not feel bad pointing mistakes because that is how I learn the best. Your genuine criticisms are highly encouraged.
Reply
Like
9
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
New Design
Jossure
-
8 Years Ago
Nothing wrong with that mate! Having taught myself to use Fusion 360 as well, I know how complex a drawing that is, so nice work.
Hanaldo
-
8 Years Ago
Yes, fusion is a great intro program. I am still learning it and the best way to learn these days is to be self-taught because you actually get to do things.
Jossure
-
8 Years Ago
I think youve done a sterling job as a first go at cad. Ive been using catia for over 17 years now and i wouldnt call myself a top designer. The automotive guys who do surfacing on bodypanels can...
scottracing
-
8 Years Ago
Thank you very much Scottracing. I do agree with you on tooling and cost. Is there a way out there to cut the cost? People I have contacted on building a prototype someday are talking of over $200K.....
Jossure
-
8 Years Ago
Looking good so far!
Warren (Staff)
-
8 Years Ago
if you want to build anything that looks semi professional then the tooling costs can easily be in the 200k upwards and thats if you have a base vehicle to start from. If you have a chassis then you....
scottracing
-
8 Years Ago
Thank you very much for the input. I have checked if there are videos explaining this out there but no luck. Anybody here has built a body using this method? Would you please share tips on how to do....
Jossure
-
8 Years Ago
there isn't really any method, to achieve car panel sized plugs from scratch, that is cheaper that wooden framing filled with foam. sure this could easily cost some thousands, but we are talking...
oekmont
-
8 Years Ago
Oekmont, Thank you very much for the idea. I am going to check them out. Yes, I know with the price of Carbon Fiber today, I am going to spend over $5000.00 on panel/body alone. I am glad there are.....
Jossure
-
8 Years Ago
A lot of metal shapers use was scott was talking about with the wooden sections to help with shaping metal. They call it a buck. It was used back when coach builders were the main car builders until....
kidpaint
-
8 Years Ago
Post Reply
Like
9
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search