Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
As said, it's not really it's design purpose. That being said, epoxy will cross link across fusion fix when used sparingly. It means it can be used in the middle of a laminate stack without it causing any structural issues.
However it is all about using it lightly. The smallest of dusting should be all you need, in which case the resin should still be able to soak through the cloth to surface to get a good bond.
From the pictures, the wood does look too smooth with a bit of shine to it. The surface should have a nice coarse key to it for maximum adhesion.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|