Using Vacuum for covering parts in CF.


Author
Message
MaksE55
M
Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)
Group: Forum Members
Posts: 5, Visits: 25
So for me the surface texture is not the problem. The problem is there is a thin coat of the film being stuck on the surface of the part. That’s the problem.
I wanted to use the vacuum back to gold down the carbon with each layer to prevent those pesky low spots that drive me inasane. Looks like that’s not possible and the release film doesn’t really work like that. Oh well
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
The part is going to come out EXACTLY the same as the surface it is in contact with. If you're putting a perforated release film on it, it's going to come out with the perforations, and likely not much gloss as those films don't tend to be glossy. As well as any creases you are getting from the bag, which tends to be inevitable given that is how you get the vacuum bag to conform to inside radii.

You could try to use a non-perforated release film like FEP or mylar release film, which will give you a good finish provided you can get any and all creases and voids out. In all honesty though, I have never had excellent results trying to get a good finish like that. There's nothing wrong with using vacuum to hold the carbon in place on complex parts, but it's less frustrating to just accept that you are still going to have to do some finishing work on the part. As long as you don't pinch the carbon in the bag, then it shouldn't take much just to sand it flat and then clear coat the parts.
Edited 8 Years Ago by Hanaldo
MaksE55
M
Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)
Group: Forum Members
Posts: 5, Visits: 25
I watched a video of a guy wrapping a intake tube he did. I spoke with him and he used th realease film right on top of the part. When it was done the film came off and the part was perfect. Meanwhile I’m over here doing the same thing over and over and still have the same result. I can do thit hand lay and all that with sanding between layers but I wanted to find a better and faster method
fibernoob
fibernoob
Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)
Group: Forum Members
Posts: 34, Visits: 134
MaksE55 - 2/26/2018 11:56:35 PM
This is actually very good for me. I have had great results with a hand layup but decided I wanted to learn how to use a vacuum for a few parts as well.
I am not trying to make a straight carbon fiber part I have done a few of those with no issue.
I have been testing different things but have not had any good luck.
I have a shifter panel for my mercedes, I laid the carbon fiber over it and used a glue to hold it all in place. next I used West System epoxy resin to wet everything out. Then placed a Perforated Release Film over my part and then the vacuum bagging over that. taped everything down and sucked the air out. pressure held very nicely so no issue there. However when I pulled the part out today (sat overnight) it almost looks like the release film left a layer on film on the part. I have had this happen to me twice so far. Its driving me a little crazy at this point. Can I get some pointers?

I have tried some parts with various films and get the same issue and some creases too. 

With peel ply I get the texture on the surface but no excess resin.   

I have seen on some videos the use of a plastic film that stretches to the part. (I think Matthieu Libeert  uses it on his videos for the mask skinning tutorials).. maybe this can be the solution.


MaksE55
M
Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)
Group: Forum Members
Posts: 5, Visits: 25
This is actually very good for me. I have had great results with a hand layup but decided I wanted to learn how to use a vacuum for a few parts as well.
I am not trying to make a straight carbon fiber part I have done a few of those with no issue.
I have been testing different things but have not had any good luck.
I have a shifter panel for my mercedes, I laid the carbon fiber over it and used a glue to hold it all in place. next I used West System epoxy resin to wet everything out. Then placed a Perforated Release Film over my part and then the vacuum bagging over that. taped everything down and sucked the air out. pressure held very nicely so no issue there. However when I pulled the part out today (sat overnight) it almost looks like the release film left a layer on film on the part. I have had this happen to me twice so far. Its driving me a little crazy at this point. Can I get some pointers?
fibernoob
fibernoob
Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)
Group: Forum Members
Posts: 34, Visits: 134
Hanaldo - 1/20/2018 1:43:22 AM
Aha... I hadn't realised you were trying to skin the inside of that lip as well. That is always going to be a struggle.

Do you actually NEED to cover the inside of the lip? It doesn't appear to be visible once the leather boot is fitted? In which case, I would simply paint it black and trim the carbon back flush with the top of the lip.

If vacuum works for you and you can do it without getting creases in the top then stick with it, there's no reason not to. What I meant with bridging is that vacuum isn't very good at getting into the inside radii, so it tends to just fill it with resin instead. If you aren't getting that problem, then vacuum is a solution! 

Yes...

Considering the contours, lip and centre hole of the part,   I think the best way out is to cover the insde radii seperately.  



fibernoob
fibernoob
Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)
Group: Forum Members
Posts: 34, Visits: 134
Interloper393 - 1/20/2018 10:10:41 AM
Buddy your over complicating things here..
Key the part with 120 grit 
Tack spray and stick the cloth to the part,  if you push excess cloth into the whole fisn't you with be able to wrap the inside too.
Apply your first resin coat and wait for it to cure.
TrI'm excess off and apply resin coats as normal


Ok - got your point... and thanks for the tips.

But the idea was to try and get the CF into tight sports and complicated bits of the part without any lift after applying the resin.

fibernoob
fibernoob
Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)Supreme Being (334 reputation)
Group: Forum Members
Posts: 34, Visits: 134
Interloper393 - 1/20/2018 10:13:24 AM

Nice parts!  Well done.
Interloper393
Interloper393
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 90, Visits: 634
All don' without vac bags
Interloper393
Interloper393
Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)Supreme Being (690 reputation)
Group: Forum Members
Posts: 90, Visits: 634

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search