It will be tough to get off, but trust me, it does come off. I had the same problem on my first part... it was a real pain in the %&§ to get off. Try snipping it into manageable strips and try to get underneath the peel ply with a sharp knife.
In future, make sure the peel ply is over lapping the reinforcement a little, so that you have something to grab onto, to make seperation easier. It is on there tough for sure and you need to apply force to remove it, careful not to flex your part too much.
hope it helps
cheers
|