Last stage but one not a glossy finish after the polish phase


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
I suspect you have moved up to a finer grit too soon or you have got a bit of grit in your paper.  Zoomed in you can see a lot of scratches on the surface. The solution is to go back down the grits until you can remove the scratches then work back up to 1200-1500 and then polish again.  Hopefully that should solve the problem.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
LioH
L
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 3, Visits: 9
Hi,
We finally finished our BMW 3-series interior in carbon. We followed step by step the tutorial but we have in thing really strange.
Left door handle is super shiny extreme deep gloss, near-perfect gloss but the right one is not so gloss, not matte but I don't have that super shiny effect. The piece looks a bit blury and we restarted the sanding process 2 times and the first time wasn't correct enough. (From 400, 800, 1200 + polish).

We have done the same process for both piece.
What can it be ? I need you advice.
Thanks,
Lionel