Hi  I found your web site through a search engine. I am very big pole fisherman the joint on the pole our worn so I get a lot of carbon deposit on my hands during fishing. I need your help I was wondering what products you do that I can purchase to seal them back up. Urgent reply needed as I have two poles doing the same understanding I can get new parts for them as they our both over 6 years old. I don’t want to buy a new pole until I haveat least tried to seal then. I have tried the products that fishing companysell but these was off during use. Hoping you deal with carbon a lot you willhave products to seal and I can get a smooth finish on the to last a lotlonger.

 

 

If you can help send me a list of items so I can order as soon as possible. Cheers I hope you can help me.

 

 

Could a product like this seal the carbon for me EL2 Epoxy Laminating Resin


Edited 14 Years Ago by Mark Dunkley
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search