Manual Vacuum Pump?
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Junior
Junior
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 73,
Visits: 473
I've been researching cheaper ways to get into resin infusion without having to splash out on an expensive vacuum pump.
Would a manual pump like this work?:
https://www.ebay.co.uk/itm/Engine-Oil-Brake-Fluid-Extractor-Removal-9L-Sump-Transfer-Vacuum-Hand-Pump/172659264201?epid=2164769182&hash=item28334b4ac9:g:I5MAAOSwBt5ZD-Xf
Some people who make RC planes use hand brake bleeder kits like this one:
https://www.ebay.co.uk/itm/HAND-VACUUM-PUMP-HELD-BRAKE-BLEEDER-TESTER-SET-BLEED-CAR-MOTORBIKE-BLEEDING-KIT/391718817400?epid=595953556&hash=item5b3442ce78:g:c48AAOSwB-1YuE1W
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Manual Vacuum Pump?
Junior
-
9 Years Ago
An interesting idea It feels like the brake test equipment might offer the best fittings etc. to obtain a good seal but, I'm guessing, that it'd take ages on anything but a small mould to extract th...
MarkMK
-
9 Years Ago
I totally recommend buying a cheap rotary vane pump. The two options you linked are -at least in my opinion- not suited for vacuum infusion. The first one does not show an achievable end pressure (bu...
oekmont
-
9 Years Ago
Thanks for the comments guys. I guess it's because what I want to do will be a one-off so it's seems expensive to shell out on all the equipment. I find it hard to find secondhand equipment, there...
Junior
-
9 Years Ago
Infusion is obviously not the ideal method for one off projects. Keep in mind, that the costs of a failed part easily exceeds the difference to a cheap pump. Especially if you sell it afterwards.
oekmont
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search