WindingMX
W
WindingMX
posted 8 Years Ago
ANSWER
HOT
Topic Details
W
Group: Forum Members
Posts: 4,
Visits: 26
Hi fellow members
Greatings from Denmark
My interest is carbonparts for motorsports
Thanks for having onboard :-)
Cheers
Kasper Winding
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Danish member
WindingMX
-
8 Years Ago
Hi! Welcome to the forum .. from another Danish member :-) I live just north of Aarhus, and work mostly on CF parts for motorbikes. (Specials, one-offs, some skinning) I use mostly infusion and som...
Dravis
-
8 Years Ago
Hejsa :-) Thats perfect, thinking about starting with carbon infusion but also considering trying prepreg. My plan is to buy the easy composites oven. Dravis, do you use a carbon/kevlar combo for...
WindingMX
-
8 Years Ago
Hi Kasper! Yes I have used several combinations of fabric, both pure Carbon , pure kevlar and mixed fibres. I normally plan ahead when it comes to fasteners in the parts, and infuse them in place,...
Dravis
-
8 Years Ago
Welcome to the forum!! A mix of carbon kevlar can be a good combination on these bike parts as it adds to abrasion resistance but still has some stiffness.
Warren (Staff)
-
8 Years Ago
Hi Warren Yeah a mix best i think. But we will do a RL test between the different blends on one of our mx bikes. (Carbon only, kevlar only and a mix).Was thinking about making some high-grade alu...
WindingMX
-
8 Years Ago
Hi Any chance that you could sent me a link to the carbon/kevlar product you would use for our mx parts? Should it be carbon/kevlar twilled layers or layers of seperat carbon and kevlar. ? Cheers...
WindingMX
-
8 Years Ago
Hi, from one more danish member. I live nearby copenhagen. I have found many good hints in this forum. during my ongoing kayak building project. Right now I am looking for an article by Dravis, wher...
Almand
-
8 Years Ago
Hi Almand, I do not think I have written about the PVA release coating, since I do not use it at all. But, I may have commented on it in some thread.
Dravis
-
8 Years Ago
Hi Dravis, Thank for replik anywayBest retarderede Keld
Almand
-
8 Years Ago
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search