Group: Forum Members
Posts: 3,
Visits: 18
|
Hi there, Just wondering which release agent would be good for two applications: 1) a barrier between two fiberglass layers - i.e. for stopping the two halves of a jacket mould over silicone 1 part mould from sticking together
2) a release agent between the silicone mould and the lay up fiberglass inside this mould to make a cast. I want the surface of the caset to be very high gloss so I am using gel coat with wax to make a top coat. I don't want the surface of this coat to be tainted by the release agent.
Would Number 8 Wax work for both applications or should I use Number 8 Wax for release agent in between the two halves of the jacket mould and Cil silicone release spray for laying up the fiberglass in the silicone mould? I don't want the release agent to affect the surface of the fiberglass resin topcoat.
|