Skinning


Author
Message
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
It is likely to leave you with lots of extra work as the surface will end up being a rough peel ply finish, thus needing the addition of another layer of resin to and more sanding and polishing to make it smooth.  Some rare occasions where the shape is very complicated, the vacuum might help hole the fabric in the right place.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
111mattin111
111mattin111
Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)
Group: Forum Members
Posts: 67, Visits: 910
When skinning a part can you resin infuse it rather than brushing on the resin?
I'm reinforcing a part in carbon so will have a barrier around to lay bagging ect.

Thanks 