By 111mattin111 - 8/23/2017 1:44:08 PM

When skinning a part can you resin infuse it rather than brushing on the resin?
I'm reinforcing a part in carbon so will have a barrier around to lay bagging ect.

Thanks 
By Warren (Staff) - 8/23/2017 3:33:26 PM

It is likely to leave you with lots of extra work as the surface will end up being a rough peel ply finish, thus needing the addition of another layer of resin to and more sanding and polishing to make it smooth.  Some rare occasions where the shape is very complicated, the vacuum might help hole the fabric in the right place.