Vinz
Vinz
posted 8 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 7,
Visits: 57
Hi all!
I'm looking to find an easy way to cut the excess material on a cured part, without having a lot of dust as cutting with Dremel?
Does anyone know any laser pen or something like that? Or some tips to help me cut?
Thanks in advance
Vinz
Vinz
www.carbonara-tech.ch
Reply
Like
3
Reply
Vinz
Vinz
posted 8 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 7,
Visits: 57
Thanks for your answer.
I will invest in a downdraft table I think.
Vinz
www.carbonara-tech.ch
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Cutting excess on cured carbon fiber sheet
Vinz
-
8 Years Ago
There isn't really any easy way to trim the edges. If it was flat sheet, you could CNC waterjet cut it which is a good hands free way of doing it. Laser cutting does not work well as the temperature....
Warren (Staff)
-
8 Years Ago
Thanks for your answer. I will invest in a downdraft table I think.
Vinz
-
8 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search