There isn't really any easy way to trim the edges. If it was flat sheet, you could CNC waterjet cut it which is a good hands free way of doing it. Laser cutting does not work well as the temperature needed to cut the carbon means it melts the resin so the edges are not very neat.
Using a downdraft table or similar vented extraction system makes the whole process much neater as the dust is removed as it is produced.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|