I'm looking to find an easy way to cut the excess material on a cured part, without having a lot of dust as cutting with Dremel?
Does anyone know any laser pen or something like that? Or some tips to help me cut?

Thanks in advance

Vinz



Vinz
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
There isn't really any easy way to trim the edges.  If it was flat sheet, you could CNC waterjet cut it which is a good hands free way of doing it.  Laser cutting does not work well as the temperature needed to cut the carbon means it melts the resin so the edges are not very neat.

Using  a downdraft table or similar vented extraction system makes the whole process much neater as the dust is removed as it is produced.



Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search