Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Projects
»
Motorsport, Vehicle Design and Modification
»
make a low spoiler bumper
make a low spoiler bumper
Post Reply
Like
6
make a low spoiler bumper
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
+cosworth
+cosworth
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 19,
Visits: 142
h ll mates
I am thinking about making a spolier to the front bumper of the car, but I have some questions on material use? you have to be flexible, you have to hold the outside temperature of 40 degrees or more in the Sun and not buckling by the temperature, the dimensions of the spolier is long 1300 mm and 200 mm in height but the thickness is 3 mm and should be black. I thought about the px90 or ef80 xencast.
I need your help
thanks
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
make a low spoiler bumper
+cosworth
-
9 Years Ago
If you are looking to cast it, then PX90 might be suitable as a casting resin. EF80 is a...
Warren (Staff)
-
9 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search