I have access to a CNC mill with which I intend to mill out moulds using MDF.

I am aware of the issues regarding MDF swell and I'm looking into figuring out how to seal it and I have a few options.

1. Using a sanding sealer/shellac to seal the milled edges and then polish until as smooth as possible

2. Use Epoxy resin to infuse the milled edges and then polish until as smooth as possible once hardened

The third I am unsure about as to whether it will work

3. Using Epoxy tooling Gelcoat to seal the milled edges create the mould surface

I'm looking to make as precise a mould as possible without resorting to metals or plastics for mould creation(as the Mill i have access to is not super great as it is a DIY build)

I'm very new to all of this sort of stuff and would appreciate any comments or suggestions as to how to proceed with MDF if at all.

Thanks
Tony2125
Tony2125
Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)Supreme Being (131 reputation)
Group: Forum Members
Posts: 12, Visits: 59
Hello

There a some material specifically design to build molds without going to aluminum or steel
I am not sure whether you can start from MDF or not
I think it also depend to the technique you will use , infusion or preg , if the mold needs to resist to temperature 
Joel Illerhag
Joel Illerhag
Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)Supreme Being (134 reputation)
Group: Forum Members
Posts: 14, Visits: 37
I would also like to have an answer to this question about making the mdf sealed.
I guess epoxy would work?
My model is very big so I can not afford to buy epoxy boards.

Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Maybe you could epoxy seal, sand lightly and then spray a polyester pattern coat primer thick. Then cnc machine again. Sand and it ready.