posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
Thanks for the info warren its definitely worth a try with the fusion fix. I think theres something similar at work so will try that out and let you know how i get on.
Cheers
Reply
Like
9
Warren (Staff)
Warren (Staff)
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 2.5K,
Visits: 8.5K
If you go for
Fusion Fix GP
, it is epoxy compatible, so although not dissolved, it does cross link meaning that from a mechanical perspective, a typical careful application on the surface and between fabric layers will not cause you any structural issues.
From the cosmetic perspective, you will likely need to clean the surface to remove the spraytack after demould. This will leave slight surface marring that as long as you were very sparing in its use, can be lightly polished out.
Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Tags
adhesive
Fusion Fix
spray tack
Reply
Like
8
scottracing
scottracing
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 460,
Visits: 5.2K
Hi all, I need some assistance on Infusing a part as its a dry substrate that I'm infusing and not a composite. I need to apply peel ply to it prior to a vac infusion at room temp using an epoxy resin system.
The part to be infused is quite complex in geometry and I was thinking of using spraytac or fusion fix to do so, but I've heard that epoxies don't dissolve it? Is this true?
Any help greatly received.
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search