RyanParle
RyanParle
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 20,
Visits: 1.2K
I've been toying with the idea of making a carbon fibre rocker cover for my A series engine, the main body should be easy enough, but I'm a bit stuck on what to do for a filler neck. I think trying to produce a neck from composite would be difficult to do & potentially be quite weak, so this leaves me with the option of using an off the shelf aluminum weld on filler neck.
What would be the best way of fixing it in place?
Could I insert the filler neck in the mould then lay up the composite around it & cure the whole lot in the oven?
Or would I be better off bonding the neck in after curing the composite part?
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
pre preg rocker cover with aluminum filler neck.
RyanParle
-
9 Years Ago
The easiest way would generally be to bond it into place from underneath. You could certainly...
Warren (Staff)
-
9 Years Ago
Thanks Warren. There are two types of filler necks that I am considering, one type is a length of...
RyanParle
-
9 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search