Hi all,I've been lurking and searching for an answer but just can't find any.

I'm replicating the process of the bonnet making tutorial.
But can PU18 be a substitute for PT326 in that same application?
There are a few bits of info here and there but no comparisons of the two.

From what I can tell it should work, but hate to have the skin flying off at speed if I'm wrong :o

Thank you!

Richard
Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The PU18 will bond the bonnet no problem.  However it is a semi-flexible adhesive meaning the join is semi-flexible.  With a large enough bead, the bond strength will be fine for most skin to frame applications.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
joochrs
joochrs
Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)Supreme Being (77 reputation)
Group: Forum Members
Posts: 5, Visits: 46
Thank you, Warren!
I can sleep better tonight knowing this Smile
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search