Hi all,I've been lurking and searching for an answer but just can't find any.

I'm replicating the process of the bonnet making tutorial.
But can PU18 be a substitute for PT326 in that same application?
There are a few bits of info here and there but no comparisons of the two.

From what I can tell it should work, but hate to have the skin flying off at speed if I'm wrong :o