Gel Coat Spray Gun


Author
Message
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Yes, there would be no reason why you couldn't spray it. There is not a huge advantage to spraying tooling gelcoat (because it doesn't really matter how smooth it goes down) but if you want to you could spray it.

Being a filled tooling gelcoat it's even thicker than a normal gelcoat or spray gel (like the GC50) and so you might need a bigger nozzle than the already large nozzle that we supply the Gelcoat Spraying Cup Gun with.

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
wozza
wozza
Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Hi Matt,
            Is the Uni-Mould Gel Coat suitable for Spray application using your Cup Gun.

Carbon Copies Ltd
wozza
wozza
Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Hi Matt,
            Thanks for the quick reply. I can now order my new compressor.

Carbon Copies Ltd
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi,

Yes, certainly, we recommend running the our Gelcoat Spraying Cup Gun at between 60 to 100. You'll need about 5.8cfm @ 80psi.

--Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
Edited 14 Years Ago by Matt (Staff)
wozza
wozza
Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)Supreme Being (8.3K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Do you have the Air requirements (CFM) for your Gel Coat Spray Gun.
Thanks in advance.

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search