Talk Composites - The Forum for Advanced Composites

Gel Coat Spray Gun

http://www.talkcomposites.com/Topic2287.aspx

By wozza - 7/17/2012 12:02:54 PM

Do you have the Air requirements (CFM) for your Gel Coat Spray Gun.
Thanks in advance.
By Matt (Staff) - 7/20/2012 7:41:34 AM

Yes, there would be no reason why you couldn't spray it. There is not a huge advantage to spraying tooling gelcoat (because it doesn't really matter how smooth it goes down) but if you want to you could spray it.

Being a filled tooling gelcoat it's even thicker than a normal gelcoat or spray gel (like the GC50) and so you might need a bigger nozzle than the already large nozzle that we supply the Gelcoat Spraying Cup Gun with.

All the best, Matt