using gel coat with resin infusion
using gel coat with resin infusion
Post Reply
Like
6
using gel coat with resin infusion
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
ajb100
ajb100
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
hi guys,
this is my first question here so any help would be much appreciated.
i've been using resin infusion to make bits and pieces for a while but now i want to make something shinier.
i wanted to use a clear gel coat and then use RI to produce a part but it had always been my understanding that you need to apply the resin when the gel coat was tacky.
watching the EC bonnet video, the gel coat is sprayed on and then sanded so obviously its dry, but i wanted to check before i try it.
if i use the EC epoxy gel coat (
https://www.easycomposites.co.uk/epoxy-bonding-polyester-gelcoat-clear
), let that dry and then lay the carbon etc down, it should all bond and work ok?
i take it the resin will re-activate the gel coat enough to bond?
Thanks
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
using gel coat with resin infusion
ajb100
-
14 Years Ago
Check this out: https://www.easycomposites.co.uk/clearpol-iso-npg-clear-polyester-gelcoat
Carbon Tuner
-
14 Years Ago
That's perfect, thanks a lot! Just a shame it's out of stock!
ajb100
-
14 Years Ago
Isn't Polyester the weakest of the esters?
Anarky
-
14 Years Ago
in structural terms it can be, but a gelcoat is not a structural usage of the polyester so its...
Warren
-
14 Years Ago
so to make it easy, the reinforcement would have to be laid down and infused/vaccuum bagged just...
mwr2452
-
14 Years Ago
follow the video. they leave it to fully cure before laying up the carbon.
Warren
-
14 Years Ago
Because there is no real UV protection with epoxy as the final finish I know that a automotive clear...
fgayford
-
14 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search