Yeh use spray adhesive like 3M Super 77 or Aerofix or FusionFix or one of those. Just be VERY sparing with your application, it will affect the finish of your part. 
Almand
Almand
Supreme Being (474 reputation)Supreme Being (474 reputation)Supreme Being (474 reputation)Supreme Being (474 reputation)Supreme Being (474 reputation)Supreme Being (474 reputation)Supreme Being (474 reputation)Supreme Being (474 reputation)Supreme Being (474 reputation)
Group: Forum Members
Posts: 19, Visits: 108
Hi,

If I want to use carbon fiber as first layer (no gelcoat), could you recommend a contact spray or something else to fix the carbon, so it would stick to the mould and be in place until infusion, but not so fixed that it´s impossible to move/slide the carbon in right position?

The mould are for a 5 meter long racing kayak, it´s prepaired with 2 times wax, and 6 times Easycomposit release agent.

Best regards
Keld
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search