Group: Forum Members
Posts: 592,
Visits: 1.9K
|
I'm going to do the exact same thing this winter .. I have two CF exhausts om my Ducati ST4S .. They are very dull looking after almost 10 years on the roads
I planned on taking the cans apart and refinishing them with EC XCR coating .. I've measured the outside temperatures on the cans and they are never above 80 - 90 centigrade, so the XCR will work just fine.