By garyt1963 - 11/22/2016 9:17:57 PM

Hi



New to all this  Smile  ..........
I have a  motorcycle with a carbon fibre exhaust sleeve which over the years has lost its shine, 
i have tried to power buff it back but it hasnt been successful... is there a product i can apply to bring back the sheen ?

Thanks in advance

Gary
By Dravis - 11/28/2016 11:08:56 AM

I'm going to do the exact same thing this winter ..
I have two CF exhausts om my Ducati ST4S .. They are very dull looking after almost 10 years on the roads

I planned on taking the cans apart and refinishing them with EC XCR coating  .. 
I've measured the outside temperatures on the cans and they are never above 80 - 90 centigrade, so the XCR will work just fine.