Group: Forum Members
Posts: 1,
Visits: 13
|
It is easy to make a two part guitar mold with resin infusion. The problem I have is then gluing the two CF pieces together. The thickness of the part is at most 1/8". Any ideas how to make a more substantial joint efficiently? I've tried methylmethacralate glue but very narrow weak joint. Thank you Paul
|