searched this forum, lots of topics about 'clouds', 'dots & spots' but couldn't find a specific answer to my question.

I use the easy comp fusion fix to stick the fibre to my pieces.  As i have a vacuum machine, for the first layer of epoxy (EL2 also easy comp) I use vacuum baging. 

after vacuum, on the first (tacky) surface i use 2 other layers of epoxy (hand layed) for thickness.

Now, in the last pieces, I saw white dots.  it it possible that (to much) fusionfix dissolves ?  or do i need to search in the regular temperature / humidity problems?

http://www.talkcomposites.com/Uploads/Images/30bc9078-8e17-49a0-bfb1-b63a.JPG