white dots


Author
Message
VVS
VVS
VVS
posted 9 Years Ago HOT
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Yes correct haha

screen is shot on my phone and I read it as infusing then adding additional layers.
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
He is skinning, not infusing. 
VVS
VVS
VVS
posted 9 Years Ago HOT
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
can I ask why you are wet laying the back layer when you can infuse everything in one operation.
dubster
dubster
Supreme Being (163 reputation)Supreme Being (163 reputation)Supreme Being (163 reputation)Supreme Being (163 reputation)Supreme Being (163 reputation)Supreme Being (163 reputation)Supreme Being (163 reputation)Supreme Being (163 reputation)Supreme Being (163 reputation)
Group: Forum Members
Posts: 15, Visits: 126
VVS (15/08/2016)
Yes that is too much fix leaching through to the front, go as light as possible.


thought so. thanks !
VVS
VVS
VVS
posted 9 Years Ago HOT
Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)Supreme Being (1.9K reputation)
Group: Moderators
Posts: 226, Visits: 334
Yes that is too much fix leaching through to the front, go as light as possible.
dubster
dubster
Supreme Being (163 reputation)Supreme Being (163 reputation)Supreme Being (163 reputation)Supreme Being (163 reputation)Supreme Being (163 reputation)Supreme Being (163 reputation)Supreme Being (163 reputation)Supreme Being (163 reputation)Supreme Being (163 reputation)
Group: Forum Members
Posts: 15, Visits: 126
searched this forum, lots of topics about 'clouds', 'dots & spots' but couldn't find a specific answer to my question.

I use the easy comp fusion fix to stick the fibre to my pieces.  As i have a vacuum machine, for the first layer of epoxy (EL2 also easy comp) I use vacuum baging. 

after vacuum, on the first (tacky) surface i use 2 other layers of epoxy (hand layed) for thickness.

Now, in the last pieces, I saw white dots.  it it possible that (to much) fusionfix dissolves ?  or do i need to search in the regular temperature / humidity problems?

http://www.talkcomposites.com/Uploads/Images/30bc9078-8e17-49a0-bfb1-b63a.JPG