ChrisR (20/07/2016)
Good choice with getting a proper industrial PID controller, now you might as well junk the idea of bodging a home oven and just build the rest of it too


Funny you say that because after I unloaded it last night and opened it up I realized how small it is. There may be an MDF oven in the near future.  
Hanaldo
Hanaldo
Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Haha yeh I concur. The PID is the most expensive bit, the rest of my oven including element and fan/motor was only around AUD$100-150. 
ChrisR
ChrisR
Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)Supreme Being (4.2K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
Good choice with getting a proper industrial PID controller, now you might as well junk the idea of bodging a home oven and just build the rest of it too
Motorious
Motorious
Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)
Group: Forum Members
Posts: 11, Visits: 99
Just to avoid the headache, I went ahead and snatched a killer deal on an RKC FB400BigGrin. No time to mess around with controllers, I got carbon fiber parts to make! With this controller i can do ramp/soak as needed so with it and a constant recirculating fan (have not sourced yet), I should be able to get good finishes.

 
Motorious
Motorious
Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)
Group: Forum Members
Posts: 11, Visits: 99
morepower (01/07/2016)
You also need to think about how fast it would heat up.. You do need a controlled ramp rate if you only have a simple PID controller. Some may not agree but I have seen a massive difference in finish with a higher ramp rate than the 1 degree every 90 seconds I currently run. I have also seen issues with a temp difference as little as 5 degrees too..  So make sure you check the oven has even heat in multiple locations through the oven and no hot or cold spots. A higher rate of flow from the fan would help if the air flow is not great. My oven recirculates the air once every 12 seconds according to the claimed airflow on the fan. This creates enough turbulence to make the oven have a more even temp throughout.   


On the subject of controlled ramp rate... I got the SSR and TA4-SNR PID wired and I was messing around with the settings and have realized that I cant control ramp rate with this setup. I can adjust the proportional band which does cause the output to the ssr to cycle on/off but only when it gets reasonably close to the setpoint. if it is say 50 degrees away from the setpoint or more, I haven't figured out a way to change the duty cycle (I dont have an oscilloscope, im just looking at an LED). I am guessing I should have bought a different PID but I'm cheap and went with the $25 one. To get around this and still use the cheapo PID, I was thinking of adding an external circuit inside the box that would intercept the on/off voltage coming from the PID. Then, when the PID is trying to go full blast with a constant 12V out, the auxiliary circuit would turn the signal into a PWM signal that I could control with say a simple potentiometer. Being a non-electrical engineer, I am not sure what would happen to the PID's ability to autotune or what the effect would be when the oven gets close to the setpoint and the pid starts cycling. I was thinking of trying it using a 555 timer based circuit like this one: DIY PWM

I have also seen SSR's that are made to have a potentiometer attached and that sounds like it might also work...
Dravis
Dravis
Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)Supreme Being (7.7K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
there are two types of ordinary household ovens.. the "Hot Air" oven, and the traditional type with no fan-

For your purpose, a "hot Air type" would be most convenient .. they almost always have a circular fan at the back of the oven.

If there is no fan ibn the oven, you will probably need to install one to circulate the air to maintain an even temperature.

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Motorious
Motorious
Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)
Group: Forum Members
Posts: 11, Visits: 99
hmm. I wonder if the oven im looking at has a fan already. Is that a standard feature or is a circulation fan something i will need to install myself? Also, im wondering if one PID could handle controlling both the SSR for the element(s) and a relay for the fan.
morepower
morepower
Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)Supreme Being (2.5K reputation)
Group: Forum Members
Posts: 242, Visits: 1.2K
You also need to think about how fast it would heat up.. You do need a controlled ramp rate if you only have a simple PID controller. Some may not agree but I have seen a massive difference in finish with a higher ramp rate than the 1 degree every 90 seconds I currently run. I have also seen issues with a temp difference as little as 5 degrees too..  So make sure you check the oven has even heat in multiple locations through the oven and no hot or cold spots. A higher rate of flow from the fan would help if the air flow is not great. My oven recirculates the air once every 12 seconds according to the claimed airflow on the fan. This creates enough turbulence to make the oven have a more even temp throughout.   
Hanaldo
Hanaldo
Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)Supreme Being (31K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Just make sure the PID controller you get can directly switch a SSR. Many of the Chinese ones on ebay say they can use a SSR or even come with one, but then require you to do some minor rewiring inside the PID to make it work. 

Not major if you know your resistors from your capacitors, but unexpected problems are a pain in the ass.
Motorious
Motorious
Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)Supreme Being (161 reputation)
Group: Forum Members
Posts: 11, Visits: 99
on second thought, with the price of those chinese PID controllers im finding, it would be silly to waste time with the arduino! Maybe another project later on BigGrin