Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Pattern and Plug Making
»
High temp chipboard tooling
High temp chipboard tooling
Post Reply
Like
4
High temp chipboard tooling
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Fasta
Fasta
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
I have done some very simple shapes using MDF. I also face the MDF with laminex/bench laminate bonded with epoxy.
Usual semi perm release system and 100C cook. Works perfect for me.
Fastacraft Facebook page
Reply
Like
4
Composite non-genius
Composite non-genius
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 6
Hi all,
Does anyone have an opinion on using a melamine/chipboard mould for a prepreg cook up to 120deg.?
Same question using plywood, mdf and OSB board.
I intend on using chipboard but am not sure what the mould stability will be like. Not very complex tooling, just some long straight battens in a U-section.
Not using an autoclave.
Look forward to your thoughts.
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search