Hi all
Complete newbie to all of this, but have (foolishly?) decided to try and build the world's first carbon fibre racing punt.
This is a vessel that will be 9 metres long, 600mm wide, and 250mm deep, built in two identical halves, so that I can put it on a roof rack.
Full details are on my website www.carbonpunt.org.uk but I have a lot of questions to ask.
Firstly: I would like to lay up one half at a time, in pre-preg, with closed cell foam as a filler. Do I need to add extra resin to the pre-preg to 'glue' the closed cell foam into the 'sandwich'?
Second: I would like to make and cure some of the components before final assembly of the complete hull half. Is this possible to add pre cured parts and cure them for a second time, without affecting the strength of the finished items?
Third (and last for the moment): I need to make a hinge/joint for the two halves, and was thinking of using nylon 6 machined components. What is the best way to join this to the carbon hull?
Thanks in advance for your time and comments
PuntDom
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search