Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
surface problem
surface problem
Post Reply
Like
2
Prev
1
2
Jump To Page
surface problem
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Hanaldo
Hanaldo
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Are you wet laying or infusing?
Either way, not enough resin and too much air are your problem.
Reply
Like
3
SUPERTIA
SUPERTIA
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 8,
Visits: 65
Hi guys, this is my first post.. i used the search button, but i haven't found my answer. When i demold my pieces in 70% of cases i have this problem, air on surface. I do this pieces for cosmetically use, so i'm expect them are perfect.. Can u help me? Here pics of the result
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Prev
1
2
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search