As above, recycle the offcuts, where possible. Even bits of tow can be used for localised reinforcement in a mould or part. The tiny scraps can be used to make a "filler paste" or used with some resin during mould making to smooth out some sharp corners when laying up the thicker layers of backing fabrics onto a mould.