Perhaps it's to do with being a bit new at this game but....
Every time I do an infusion or cut some carbon I seem to end up with lengths of carbon tow laying around on the floor
Does anyone have any interesting uses for this otherwise waste material?
I have tried to wrap some around a bar to make a ring which kind of worked after some sanding and clear coat.
|