Author
Message
carbon man
carbon man
posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Awaiting Activation
Posts: 86,
Visits: 1.2K
Hi, i have used the search and it's been very helpfull with other self builds, but couldn't find a list of things to buy.
I will have everything for outside of the oven, I just need a list of fixings/temperature controls etc..
And where best to purchase.
And any advice will be greatfull.
Thanks
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Oven build list
carbon man
-
10 Years Ago
eBay is your friend... It depends on oven size and where you want to place the fan etc...
morepower
-
10 Years Ago
EBay for the fan motor, oven element, Solid State Relay and thermal switch. For the SSR, you want...
Hanaldo
-
10 Years Ago
Thanks for the reply, does it matter what size element and fan I use? I plan on making the oven...
carbon man
-
10 Years Ago
Fan doesn't matter, just any oven fan. Element, just get a 2000w one. Your oven is roughly the same...
Hanaldo
-
10 Years Ago
Thanks, did you do a post when making yours? Or have any photos /tips before I start. Cheers
carbon man
-
10 Years Ago
[quote][b]carbon man (02/04/2016)[/b][hr]Thanks, did you do a post when making yours? Or have any...
Hanaldo
-
10 Years Ago
Will throw up a thread with photos a bit later for you. Have been meaning to do it for awhile so...
Hanaldo
-
10 Years Ago
There was a good guide in the practical guide to composites book, could take a photo or scan of it?...
scottracing
-
10 Years Ago
Just last night finishedbuilding my oven with the advice of theeasy compositesteam. Its a VERY...
andygtt
-
10 Years Ago
Just last night finishedbuilding my oven with the advice of theeasy compositesteam. Its a VERY...
andygtt
-
10 Years Ago
Hi, my name is Alessandro and I can sell you all the equipments you need to build your own oven...
carbonrace
-
10 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search