It shouldn't. Parts like that are generally press moulded, so they are designed with enough taper to get them out of the mould. 

You will have to follow your own instincts a bit, as it's very difficult to tell from those photos whether or not you've got a lock. My impression, looking at those photos and knowing how they were likely made, would be that they will come out of the mould ok. If you don't feel confident in that then it's always better to do a split mould instead. 

111mattin111
111mattin111
Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)
Group: Forum Members
Posts: 67, Visits: 910
Also here where the inner and outer meet
http://www.talkcomposites.com/Uploads/Images/9e27015c-0b04-41ef-b5e9-0dab.jpg
111mattin111
111mattin111
Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)
Group: Forum Members
Posts: 67, Visits: 910
HI I'm about to start making moulds of my car doors and was wondering when I do the mould of the inner skin  (door card side) will it mechanically lock as the two sides aren't tapered 

http://www.talkcomposites.com/Uploads/Images/61183e79-886c-49cd-aa51-4f0f.jpg


http://www.talkcomposites.com/Uploads/Images/f9842fe6-5562-43fb-b46d-11b6.jpg
http://www.talkcomposites.com/Uploads/Images/b1b42278-734d-40fd-a93c-8707.jpg
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search