Not done much on account of my sciatica.Made a start on the flanges,
hot glued a strip of correx around the inside of the tank,then used
filleting wax to smooth the edge,then cut and hot glued the flanges
on,more filleting wax will be used to smooth the joints.Looks dodgy
underneath but as that's not the important part,not to bothered,it does
the job.

http://www.talkcomposites.com/Uploads/Images/6ffbe32d-89c5-4857-afbd-b29d.jpghttp://www.talkcomposites.com/Uploads/Images/282f9815-7e9a-4e9e-b0df-0d20.jpghttp://www.talkcomposites.com/Uploads/Images/22f1c1ff-c525-4e39-9858-7ace.jpghttp://www.talkcomposites.com/Uploads/Images/8a09e141-34d5-4372-a3cd-ac25.jpg
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search