By Paul M - 2/28/2016 1:46:10 PM
Before I put the flanges on the tank to make the mould,does it matter if they are at 90 degrees or 180 degrees to the edge for infusion bagging
Cheers Paul
|
By Paul M - 4/4/2016 5:19:13 PM
Not done much on account of my sciatica.Made a start on the flanges, hot glued a strip of correx around the inside of the tank,then used filleting wax to smooth the edge,then cut and hot glued the flanges on,more filleting wax will be used to smooth the joints.Looks dodgy underneath but as that's not the important part,not to bothered,it does the job.
  
|
|