The "Moto-GP"  Carbon brake rotors are like the ones used on cars .. They are "CC" or Carbon-Carbon" sintered material -
The Axis CMC rotors are "Ceramic Matrix Carbon" a very different material that does not need to be hot to function like the CC MotoGP rotors --
So you can use them on road bikes as well -- If you are willing to pay - BigGrin

They are made by laying up carbon weave in a wet ceramic matrix, then baking the "cake" in a very hot oven under high pressure . Like making Clay pottery.. only a bit more "high tech"Cool

The first two generations of CMC brake rotors were not strong enough in the thin dimensions used on bikes .. they are used in Hyper Sports Cars where the dimensions are much bigger /thicker

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
tomzi1234
tomzi1234
Supreme Being (491 reputation)Supreme Being (491 reputation)Supreme Being (491 reputation)Supreme Being (491 reputation)Supreme Being (491 reputation)Supreme Being (491 reputation)Supreme Being (491 reputation)Supreme Being (491 reputation)Supreme Being (491 reputation)
Group: Forum Members
Posts: 40, Visits: 500
i knew about MotoGP carbon discs, but those looks diferent, not like plain weave carbon fibre.
and those looks like normal carbon fibre,
that's why the question.

thank you for lighten me up Smile
Dravis
Dravis
Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)Supreme Being (8.6K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
The Carbon-fibre brake rotors are "BrakeTech"  AXIS/CMC  -- they are very real -- and very light -- w00tCool

I would like to be able to afford a set for my MV Agusta ..  Smooooth

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
tomzi1234
tomzi1234
Supreme Being (491 reputation)Supreme Being (491 reputation)Supreme Being (491 reputation)Supreme Being (491 reputation)Supreme Being (491 reputation)Supreme Being (491 reputation)Supreme Being (491 reputation)Supreme Being (491 reputation)Supreme Being (491 reputation)
Group: Forum Members
Posts: 40, Visits: 500
nice work.

i like wheels Smile

disk brakes? are they only for show or actually works ?
davro
davro
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
Looks real nice !

Like the layup pattern on the front fairing around the light and indicators, pre pregs allow for interesting layup patterns.

What moulding system are you using for your prepreg moulds out of interest, I have only played around with resin infusions ...



David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


Edited 10 Years Ago by davro
racecomp
racecomp
Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)
Group: Forum Members
Posts: 5, Visits: 10
http://www.talkcomposites.com/Attachment1127.aspxhttp://www.talkcomposites.com/Attachment1126.aspxhttp://www.talkcomposites.com/Attachment1124.aspxSome of my carbon bikes and other parts that RaceComp make, all Autoclave cured pre-preg.
Attachments
triumph-1 1.jpg (2K views, 615.00 KB)
triumph-2.jpg (988 views, 375.00 KB)
100_3844.jpg (2.2K views, 188.00 KB)
100_3866.JPG (2.2K views, 784.00 KB)
100_1985 RC.jpg (974 views, 192.00 KB)
100_2822 RC.jpg (998 views, 223.00 KB)
Edited 10 Years Ago by racecomp
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search