valerio.polenta
valerio.polenta
posted 11 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 24
Hello,
I'm building some pregreg components as part of a university project. For brevity, I will skip details, I just tell you that so far I've built some "pipes" with a kind of D-section (and a taper angle to facilitate mould extraction). The picture shows the mould, the prepreg shapes and the final part.
Now, what I want to do is to attach 2 of those pipes together by placing them adjacent along the flat part and adding an outer layer of prepreg, like in this sketch:
My question is: can the two inner pipes go into the oven again? They already underwent a cycle of 4 hours (
1hr @ 50'C, 1
hr @ 60'C,
1hr @ 70'C,
1hr @ 120'C). I'm using
Easy-Preg 240g 3K Surfacing Prepreg
and
Vari-Preg 400g 12K
.Backing Ply. I wonder if the mechanical properties deteriorate after a second cycle like that.
Thanks,
Valerio
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Can prepreg parts be cured again?
valerio.polenta
-
11 Years Ago
by seeing your curing cycle they will probably soften a bit when you put them back into the oven....
matthieutje65
-
11 Years Ago
Give the original parts a higher post cure once de moulded to get a higher tg an you should be ok on...
f1rob
-
11 Years Ago
I once had left out two layers of prepreg in an autoclaved piece. I ground the surface with 36 grit...
fgayford
-
9 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search