3D printing patterns/moulds


Author
Message
67redrocket
67redrocket
Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)
Group: Forum Members
Posts: 49, Visits: 486
I have used www.shapeways.com for 3d printing a couple of times. And I wonder if I can use this to print patterns or moulds. Does anyone have experience with printing patterns/moulds?

The material shapeways use is called PA 2200

worthidlj
worthidlj
Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)Supreme Being (82 reputation)
Group: Forum Members
Posts: 13, Visits: 1.2K
The issue with 3D printed parts is they are NOT sealed surfaces (even the SLS, SLA, DLP variants).

The way to get around this is to coat the surface/ soak the part (in a sealable bag if part is small enough) with epoxy and sand smooth then I think from there it is the usual moulding process.

This is my understanding of it, but happily to be corrected.




Cheers,

David
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
its an application that im looking into at work. I have used sls nylon before but we had to seal the tools after we had wet sanded them smooth.
I know many companies and motorsport especially are looking into it, if things progress as work I will give an update on the materials used and what needa to be done post process
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
Just coat with marbokote 2002 as you would tooling block then release with whatever

can also use 712
Bean Bandit
Bean Bandit
Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)Forum Guru (70 reputation)
Group: Forum Members
Posts: 10, Visits: 136
Hi everyone,

I'm very much at the beginning of making composite parts and have just ordered some materials.

I want to make some airhorns/stacks for my car and planed to get the mould 3D printed out of ABS (Tg around 120°C) and then seal it with a thin layer of high temp epoxy.

I bought some braided cf sleeves (in combination with high temp epoxy) and will try how that works first but also got some prepreg (hence the goal to make a mould which can take 100°C or more). 

Is there anything I'm missing that would speak against my above mentioned plan (incompatability of resins, chemical reactions etc)?

If there aren't any objections I'll give it a go later this summer/early autumn. Currently temps are too high (30°C or more in my working area).

Thanks for any input. 

Bean
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search