Question,

Can the High temp resin be used in a "hot tool" process?

What I mean is, can the cure be accelerated by elevating the temperature during cure? I suspect it will increase of course, and I understand a post cure is not the same thing, but I am wondering if stable metal moulds could be used with this resin to produce a quick turn around time?

I looked at the data sheets, but could not find a list of curing times against the ambient temp.
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
alex.mc - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search